Arif, windarto (2019) KINETIKA DAN PEMBENTUKAN KERAK FERRO KARBONAT DENGAN PENAMBAHAN ZEOLIT 1500 mg dan 3000 mg. Sarjana / Sarjana Terapan (S1/D4) thesis, Universitas Muhammadiyah Semarang.
![]() |
Text
Laporan Tugas Akhir Arif Windarto (final).pdf Restricted to Repository staff only Download (2MB) | Request a copy |
|
|
Text
Jurnal Tugas Akhir Arif Windarto (final).pdf Download (1MB) | Preview |
Abstract
KINETIKA DAN PEMBENTUKAN FERRO KARBONAT DENGAN PENAMBAHAN ZEOLIT 1500 mg dan 3000 mg Arif windarto, Dr. Samsudi Raharjo, MT, MM dan Rubijanto JP., ST, MT Teknik Mesin Universitas Muhammadiyah Semarang Email : arifwindart@gmail.com ABSTRAK Proses alami dari reaksi kimia antara kandungan-kandungan yang terkandung atau terlarut di dalam air dalam suatu pergerakan sistem kerja yanga mengakibatkan timbulnya kerak sehingga terjadi kerugian di dalam sistem. Salah satunya komponennya adalah Ferro karbonat Fe2 (CO3)3. Fenomena pengerakan sering dijumpai di sistem perpiapaan industri maupun rumah tangga. Penyumbatan yang diahasilkan dari proses pengerakan menimbulkan masalah teknis maupun ekonomis. Hal ini disebabkan karena terdapatnya unsur-unsur pembentuk kerak seperti besi dan karbonat dalam jumlah yang melebihi kelarutannya pada peralatan berat. Kerak biasanya mengendap dan tumbuh pada peralatan industri seperti pada pipa pipa hidrolik alat berat. Kerak merupakan suatu deposit dari senyawa-senyawa anorganik yang terendapkan dan membentuk timbunan kristal pada permukaan suatu subtansi. Kerak merupakan suatu deposit dari senyawa-senyawa anorganik yang terendapkan dan membentuk timbunan kristal pada permukaan suatu subtansi. Hal ini disebabkan karena terdapatnya unsur-unsur pembentuk kerak seperti alkalin, magnesium, kalsium, klorid, sulfat dalam jumlah yang melebihi kelarutannya pada keadaan kesetimbangan. Kerak biasanya mengendap dan tumbuh pada peralatan industri dan rumah tangga yang mememanfaatkan pergerakan fluida untuk proses kerjanya. Kata Kunci : Ferro carbonat, Pengerakan Ferro karbonat KINETIKA DAN PEMBENTUKAN FERRO KERAK KARBONAT DENGAN PENAMBAHAN ZEOLIT 1500 mg dan 3000 mg Arif windarto, Dr. Samsudi Raharjo, MT, MM dan Rubijanto JP., ST, MT Teknik Mesin Universitas Muhammadiyah Semarang Email : arifwindart@gmail.com ABSTRACT The natural process of a chemical reaction between the contents contained in or dissolved in water in a movement of the work system which results in crust so that there is a loss in the system. One of the components is Ferro carbonate Fe2 (CO3) 3. The scaling phenomenon is often found in industrial and household systems. The blockages that result from the grinding process cause technical and economic problems. This is due to the presence of crust-forming elements such as iron and carbonates in amounts that exceed their solubility in heavy equipment. The crust usually settles and grows on industrial equipment such as heavy equipment hydraulic pipe pipes. The crust is a deposit of inorganic compounds which are deposited and form crystalline deposits on the surface of a substance. The crust is a deposit of inorganic compounds which are deposited and form crystalline deposits on the surface of a substance. This is due to the presence of crust-forming elements such as alkaline, magnesium, calcium, chloride, sulfate in amounts that exceed their solubility in equilibrium conditions. The crust usually settles and grows on industrial equipment and households that utilize fluid movements for their working processes. Keywords: Ferro carbonate, Ferro carbonate drying
Item Type: | Thesis (Sarjana / Sarjana Terapan (S1/D4) ) |
---|---|
Subjects: | T Technology > TJ Mechanical engineering and machinery |
Divisions: | Faculty of Engineering > S1 Mechanical Engineering |
Depositing User: | perpus unimus |
URI: | http://repository.unimus.ac.id/id/eprint/8556 |
Actions (login required)
![]() |
View Item |